LQ-S
UPG & LQ
LQJH PETG Shrink film
Widely used for bottle
(big diameter difference between bottleneck and body, film labeling, eg.Beverage bottles packaging, cleaning and bathing products packaging and cosmetics packaging.
LQJH PETG Shrink film
Widely used for bottle
(big diameter difference between bottleneck and body, film labeling, eg.Beverage bottles packaging, cleaning and bathing products packaging and cosmetics packaging.
PROPERTY
| UNIT | TEST METHOD | TYPICAL VALUE | |
THICKNESS |
um |
ASTM D374 |
50 | |
DENSITY |
g/cm3 |
ASTM D792 |
1.32 | |
HAZE |
% |
D1003 |
4.1 | |
LIGHT TRANSMITTANCE
|
% |
ASTM D1003 |
90.6 | |
COEFFICIENT OF FRICTION
|
us |
ASTM D1894E |
0.5 | |
uk |
0..53 | |||
TENSILE STRENGTH
|
Mpa |
ASTM D882 | M D |
50.2 |
TD |
243.6 | |||
ELONGATION AT BREAK
|
% |
ASTM D882 | M D |
408 |
TD |
42.5 | |||
SHRINKAGE (In 90℃ water for 10 sec.) |
% |
ASTM D1204 | M D |
3 |
TD |
74 |
PROPERTY
| UNIT | TEST METHOD | TYPICAL VALUE | |
THICKNESS |
um |
ASTM D374 |
50 | |
DENSITY |
g/cm3 |
ASTM D792 |
1.32 | |
HAZE |
% |
D1003 |
4.1 | |
LIGHT TRANSMITTANCE
|
% |
ASTM D1003 |
90.6 | |
COEFFICIENT OF FRICTION
|
us |
ASTM D1894E |
0.5 | |
uk |
0..53 | |||
TENSILE STRENGTH
|
Mpa |
ASTM D882 | M D |
50.2 |
TD |
243.6 | |||
ELONGATION AT BREAK
|
% |
ASTM D882 | M D |
408 |
TD |
42.5 | |||
SHRINKAGE (In 90℃ water for 10 sec.) |
% |
ASTM D1204 | M D |
3 |
TD |
74 |